H

EFD20

9

20.0±0.6

15.4±0.5

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21A

9

20.8±0.6

15.4분

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21B

9.7

21.0±0.5

15.4분

8.9±0.2

6.7±0.2

8.0±0.3

10.3±0.3

\

3.6±0.2

EFD25.6

19

25.6±0.7

19.5±0.7

11.4±0.3

9.1±0.3

9.3±0.3

12.5±0.3

0.6±0.1

5.2±0.3

EFD31

25

30.8±0.8

23.2분

14.4±0.3

8.8±0.2

11.2±0.3

15.0±0.3

0.3±0.2

4.8±0.2

EFD34

29.6

34.0±0.6

24.0±0.5

17.0±0.3

5.0±0.2

18.0±0.3

23.0±0.3

\

3.0±0.2

EFD40/45/11

60

40.5±0.7

30.0분

16.6±0.3

10.6±0.2

16.3±0.3

22.5±0.3

\

6.6±0.2

EFD40/44/8

44

40.0±0.7

29.5분

19.9±0.4

8.0±0.2

17.1±0.3

22.0±0.3

\

4.0±0.2

EFD43/53/4.4

63.6

43.0±0.8

28.5분

21.6±0.4

7.6±0.25

19.3±0.3

26.5±0.3

\

4.4±0.25

EFD43/44/3.2

49.2

43.4±0.8

33.5분

22.3±0.4

8.0±0.25

17.1±0.3

22.2±0.3

\

3.2±0.25

EFD45/50

67

45.2±0.8

33.3±0.8

24.0±0.4

7.8±0.2

18.0±0.3

24.7±0.3

\

4.0±0.2

EFD52.5

118

52.5±1.1

39분

22.5±0.4

13.0±0.3

19.9±0.3

27.0±0.3

\

7.5±0.3

 

모델

매개변수

AL±25%(nH/N^2)

N.W(g)

C1mm-1

렘

에엠2

벰3

ZP40

EFD20

1.52

47.0

31.0

1460.0

1150

7.9

EFD21A

1.57

49.3

31.0

1460.0

1400

7.9

EFD21B

1.57

49.3

31.4

1540.0

1450

8.6

EFD25.6

1.00

57.0

58.0

3300.0

2000

16.5

EFD31

0.99

68.2

69.1

4712.0

2000

23.0

EFD34

1.90

95.0

50.0

4750.0

1400

33.5

EFD40/45/11

1.02

108.8

106.5

10951.0

2300

55.0

EFD40/44/8

1.35

102.8

75.5

7750.0

1700

38.0

EFD43/53/4.4

1.14

111.3

99.8

11113.0

2000

59.0

EFD43/44/3.2

1.41

102.0

72.1

7352.0

1500

43.0

EFD45/49

1.08

108.0

97.7

10356.2

2700

60.0

EFD52.5

0.78

132.0

168.0

23250.0

2750

109.0