페라이트 PQ 코어



|
모델 |
G.W |
크기(mm) |
||||||
|
A |
B최소 |
C |
D |
E |
F |
지민 |
||
|
PQ20/16 |
15 |
20.5±0.4 |
18.0±0.4 |
8.8±0.2 |
14.0±0.4 |
5.2±0.2 |
8.1±0.1 |
12.0 |
|
PQ20/20 |
17 |
20.5±0.4 |
18.0±0.4 |
8.8±0.2 |
14.0±0.4 |
7.2±0.2 |
10.1±0.1 |
12.0 |
|
PQ26/20 |
34 |
26.5±0.5 |
22.5±0.45 |
12.0±0.2 |
19.0±0.45 |
5.7±0.2 |
10.1±0.1 |
15.5 |
|
PQ26/25 |
40 |
26.5±0.5 |
22.5±0.45 |
12.0±0.2 |
19.0±0.45 |
8.0±0.2 |
12.4±0.2 |
15.5 |
|
PQ27/20 |
34.6 |
27.3±0.5 |
22.5분 |
12.0±0.2 |
19.0±0.45 |
5.8±0.25 |
10.1±0.25 |
16.0 |
|
PQ27/25 |
41 |
27.3±0.5 |
22.5분 |
12.0±0.2 |
19.0±0.45 |
8.2±0.25 |
12.5±0.25 |
16.0 |
|
PQ27.5A/20 |
35.6 |
27.5±0.5 |
22.3분 |
12.0±0.2 |
19.0±0.45 |
5.8±0.25 |
10.1±0.25 |
16.0 |
|
PQ27.5A/25 |
41.6 |
27.5±0.5 |
22.3분 |
12.0±0.2 |
19.0±0.45 |
8.2±0.25 |
12.5±0.2 |
16.0 |
|
PQ27.5B/20 |
34.6 |
27.5±0.5 |
22.8분 |
12.0±0.2 |
19.0±0.45 |
5.8±0.25 |
10.1±0.25 |
16.0 |
|
PQ27.5B/25 |
40.6 |
27.5±0.5 |
22.8분 |
12.0±0.2 |
19.0±0.45 |
8.2±0.25 |
12.5±0.2 |
16.0 |
|
PQ32/20 |
45 |
32.0±0.6 |
27.5±0.5 |
13.4±0.3 |
22.0±0.5 |
5.8±0.25 |
10.1±0.25 |
19.0 |
|
PQ32/25 |
52 |
32.0±0.6 |
27.5±0.5 |
13.4±0.3 |
22.0±0.5 |
8.3±0.25 |
12.5±0.25 |
19.0 |
|
PQ32/30 |
62 |
32.0±0.6 |
27.5±0.5 |
13.4±0.3 |
22.0±0.5 |
10.7±0.25 |
15.0±0.25 |
19.0 |
|
PQ32/35 |
67 |
32.0±0.6 |
27.5±0.5 |
13.4±0.3 |
22.0±0.5 |
12.6±0.3 |
16.9±0.25 |
19.0 |
|
PQ32.5/20 |
46 |
32.5±0.6 |
28.0±0.5 |
13.4±0.3 |
22.0±0.5 |
5.8±0.25 |
10.1±0.25 |
19.5 |
|
PQ32.5/25 |
53 |
32.5±0.6 |
28.0±0.5 |
13.4±0.3 |
22.0±0.5 |
8.3±0.25 |
12.5±0.25 |
19.5 |
|
PQ32.5/30 |
63 |
32.5±0.6 |
28.0±0.5 |
13.4±0.3 |
22.0±0.5 |
10.7±0.25 |
15.0±0.25 |
19.5 |
|
PQ33/30 |
61.6 |
33.0±0.6 |
28.5±0.5 |
13.4±0.3 |
22.0±0.5 |
10.7±0.25 |
15.0±0.25 |
20.0 |
|
PQ35/35 |
77.6 |
35.1±0.7 |
32.0±0.5 |
14.4±0.3 |
26.0±0.5 |
12.5±0.25 |
17.5±0.25 |
23.5 |
|
PQ40/40 |
101 |
40.5±0.9 |
37.0±0.6 |
14.9±0.3 |
28.0±0.6 |
14.7±0.25 |
19.9±0.25 |
28.0 |
|
PQ50/50 |
216 |
50.0±0.9 |
44.0±0.7 |
20.0±0.3 |
32.0±0.6 |
18.0±0.25 |
25.0±0.25 |
31.5 |
|
PQM27/20 |
31 |
26.8±0.4 |
23.0분 |
11.8±0.2 |
18.9±0.3 |
6.1±0.25 |
9.5±0.25 |
17.0 |
|
PQM27/25 |
37.2 |
26.8±0.4 |
23.0분 |
11.8±0.2 |
18.9±0.3 |
9.1±0.25 |
12.5±0.25 |
17.0 |
|
PQM32/20 |
44 |
32.0±0.5 |
28.0분 |
13.6±0.2 |
22.0±0.3 |
6.5±0.25 |
10.0±0.25 |
20.8 |
|
PQM32/25 |
56 |
32.0±0.5 |
28.0분 |
13.6±0.2 |
22.0±0.3 |
8.8±0.25 |
12.3±0.25 |
20.8 |
|
PQM32/30 |
61 |
32.0±0.5 |
28.0분 |
13.6±0.2 |
22.0±0.3 |
11.2±0.25 |
14.7±0.25 |
20.8 |
|
PQM38 |
32.8 |
38.0±0.8 |
32.0분 |
14.2±0.3 |
21.2±0.5 |
3.5±0.3 |
6.5±0.3 |
26.7 |
|
CQ28/20 |
56 |
28.0±0.4 |
24.6±0.4 |
13.25±0.25 |
28.0±0.4 |
6.7±0.25 |
10.2±0.25 |
7.6 |
|
모델 |
매개변수 |
AL±25%(nH/N^2) |
N.W(g) |
|||||
|
C1mm-1 |
렘 |
에엠2 |
벰3 |
ZP40 |
||||
|
PQ20/16 |
0.605 |
37.4 |
62.0 |
2310 |
3300 |
13 |
||
|
PQ20/20 |
0.738 |
45.4 |
62.0 |
2790 |
3100 |
15 |
||
|
PQ26/20 |
0.391 |
46.3 |
119.0 |
5490 |
6100 |
31 |
||
|
CPQ26/25 |
0.472 |
55.5 |
118.0 |
6530 |
5200 |
36 |
||
|
PQ27/20 |
0.411 |
47.6 |
117.0 |
5490 |
6100 |
31 |
||
|
PQ27/25 |
0.481 |
56.8 |
116.0 |
6530 |
5200 |
36.5 |
||
|
PQ27.5A/20 |
0.409 |
48.5 |
118.0 |
5720 |
6100 |
32 |
||
|
PQ27.5A/25 |
0.491 |
57.6 |
117.0 |
6750 |
5200 |
37.5 |
||
|
PQ27.5B/20 |
0.414 |
48.5 |
117.0 |
5670 |
6100 |
31 |
||
|
PQ27.5B/25 |
0.496 |
57.6 |
116.0 |
6680 |
5200 |
36.5 |
||
|
PQ32/20 |
0.326 |
55.5 |
161.0 |
9420 |
6000 |
42 |
||
|
PQ32/25 |
0.376 |
60.6 |
161.0 |
9760 |
5500 |
48 |
||
|
PQ32/30 |
0.464 |
78.2 |
161.0 |
12600 |
5150 |
55 |
||
|
PQ32/35 |
0.546 |
85.2 |
161.0 |
13300 |
3950 |
66 |
||
|
PQ32.5/20 |
0.326 |
55.5 |
161.0 |
9420 |
6000 |
42 |
||
|
PQ32.5/25 |
0.376 |
60.6 |
161.0 |
9760 |
5500 |
48 |
||
|
PQ32/30 |
0.464 |
78.2 |
161.0 |
12600 |
5150 |
55 |
||
|
PQ33/30 |
0.471 |
79.8 |
161.0 |
12850 |
5000 |
55.8 |
||
|
PQ35/35 |
0.448 |
87.9 |
196.0 |
17300 |
4860 |
73 |
||
|
PQ40/40 |
0.508 |
102 |
201.0 |
20500 |
4300 |
95 |
||
|
PQ50/50 |
0.346 |
113 |
328.0 |
37200 |
6720 |
195 |
||
|
PQM27/20 |
0.43 |
45.6 |
105.0 |
4800 |
5000 |
28 |
||
|
PQM27/25 |
0.545 |
57.4 |
105.0 |
6050 |
4800 |
32.5 |
||
|
PQM32/20 |
0.392 |
55.9 |
145.7 |
7990 |
5500 |
40 |
||
|
PQM32/25 |
0.45 |
65.9 |
145.7 |
9596 |
5000 |
50.5 |
||
|
PQM32/30 |
0.562 |
76.7 |
145.7 |
11200 |
4500 |
55 |
||
|
PQM38 |
0.378 |
43.6 |
118.0 |
5140.0 |
5800 |
30 |
||
|
CQ28/20 |
0.312 |
46.56 |
149.2 |
6948.0 |
7000 |
48.5 |
||